VoyForums
[ Show ]
Support VoyForums
[ Shrink ]
VoyForums Announcement: Programming and providing support for this service has been a labor of love since 1997. We are one of the few services online who values our users' privacy, and have never sold your information. We have even fought hard to defend your privacy in legal cases; however, we've done it with almost no financial support -- paying out of pocket to continue providing the service. Due to the issues imposed on us by advertisers, we also stopped hosting most ads on the forums many years ago. We hope you appreciate our efforts.

Show your support by donating any amount. (Note: We are still technically a for-profit company, so your contribution is not tax-deductible.) PayPal Acct: Feedback:

Donate to VoyForums (PayPal):

Login ] [ Contact Forum Admin ] [ Main index ] [ Post a new message ] [ Search | Check update time | Archives: 12[3]4 ]


[ Next Thread | Previous Thread | Next Message | Previous Message ]

Date Posted: 22:29:06 12/12/07 Wed
Author: Thad Russell (Merry)
Author Host/IP: c-24-128-90-71.hsd1.ma.comcast.net / 24.128.90.71
Subject: Painting Advise 58 Sea Skiff

Hi, I have a new 58 Sea Skiff with plywood lapstrake hull. I has ablative anti-fouling paint but I need to paint it green again. It is now in fresh water and on a boat lift so I don't need ablative anti-fouling paint.

Can I use a stripper or will this hurt the glue and so will I have to sand it?

Does anyone recommend an undercoat of poly resin like West Systems or primer. I am not planning fiberglass. Any help or suggested sources are appreciated. Bright work is in pretty good shape. Thanks

[ Next Thread | Previous Thread | Next Message | Previous Message ]


Replies:

[> Re: Painting Advise 58 Sea Skiff -- Craig, 08:18:28 01/01/08 Tue (cpe-69-205-121-24.rochester.res.rr.com/69.205.121.24)

Thad,
I own 2 1957 sea skiffs one of which is almost done. Having just completed my hull paint I can share with you what I did.
I stripped the entire hull to bare wood by sanding. I had a problem with oil soaked areas under the engine which had gone all the way through so I put two coats of CPES on the exterior sanding between coats. This gave me a solid base coat on which to paint without fear of peeling. I then refilled all screw holes with 3m premium filler, primed with Interlux base coat then applied multiple coats of Interlux Brightside polyurethane sanding between. The result is a very hard high gloss finish that absolutely looks like glass. A long tedius process but well worth it in my opinion. Just remember, all time spent preparing the surface before painting will give tremendous paybacks.

[ Post a Reply to This Message ]
[ Edit | View ]





Post a message:
This forum requires an account to post.
[ Create Account ]
[ Login ]
[ Contact Forum Admin ]


Forum timezone: GMT-5
VF Version: 3.00b, ConfDB:
Before posting please read our privacy policy.
VoyForums(tm) is a Free Service from Voyager Info-Systems.
Copyright © 1998-2019 Voyager Info-Systems. All Rights Reserved.